Stainless steel metal is peeling away
Moderators: Brad Walker, Tony Smith
Stainless steel metal is peeling away
I am using stainless steel molds and since the first fire, they continue to peel each time afterwards. Is this common in stainless steel. It is getting into my glass. When is peels, is this the same thing as spall?
Thanks for the info.
Mike Hawkins
(hoknok)
pronounced Hock-Nock as in Brock ( for those who have asked...)
			
			
									
						
										
						Thanks for the info.
Mike Hawkins
(hoknok)
pronounced Hock-Nock as in Brock ( for those who have asked...)
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
- 
				Goldfinger
- Posts: 54
- Joined: Wed Jan 07, 2004 11:07 am
- Location: Missouri
stainless steel metal peeling away
I have seen the peeling stainless steel as you've described but only in a corrosive enviroment. Stainless steel doesn't melt until around 2500 F.
			
			
									
						
										
						- 
				Paul Housberg
- Posts: 103
- Joined: Fri Mar 21, 2003 1:08 pm
- Location: Rhode Island
- Contact:
There are different grades of stainless and some are more resistant to corrosion than others. 
You're certain they are stainless?
Are these molds specifically made for glass?
Are they flaking or are you getting crud sticking to your glass?
Can you provide details on the type of glass, firing schedule, etc.
			
			
									
						
							You're certain they are stainless?
Are these molds specifically made for glass?
Are they flaking or are you getting crud sticking to your glass?
Can you provide details on the type of glass, firing schedule, etc.

Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
you should be using some sort of fiber paper anyway with these types of molds, as the steel will shrink more than the glass, and you'll need to account for the less room inside the mold.
it's probably just not a type of stainless steel that resists spalling, if it's stainless at all.
you could use cut up shelves or tiles to make dams instead, if you wanted different sized ones than what you could get from this mold. you still have to use fiber paper with these too. if you use 1/16" paper, it's reusable a few times.
			
			
									
						
										
						it's probably just not a type of stainless steel that resists spalling, if it's stainless at all.
you could use cut up shelves or tiles to make dams instead, if you wanted different sized ones than what you could get from this mold. you still have to use fiber paper with these too. if you use 1/16" paper, it's reusable a few times.
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Does a magnet stick to it? If it does, there's a very good chance it's not stainless.SAReed wrote:I've been using these for pattern barsand have noticed peeling. I use ThinFire as a barrier so luckily it's not getting on the glass. But I was wondering what was causing it. I'm also wondering how many more uses I'll get out of them before they fall apart.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						Tried the magnet, didn't stick.  I'm sure it's stainless, but comparing it to a stainless bowl I've used for slumping that hasn't peeled, it's a lot thinner.  I'm guessing it's a poorer quality of stainless.  What really gets me is I paid $14 for each bar tray and it's probably $0.50 of stainless that's used.  I could have had a stainless cutter and bender for free and didn't take it....how was I to know I could've used it???  ](./images/smilies/eusa_wall.gif)
			
			
									
						
							](./images/smilies/eusa_wall.gif)
Stacey
			
						well I just tried the magnet and although it did not stick to the mold its self, all the particles (metal flakes) in the mold did stick to the magnet?
Anyway, I am sure these are not the quality stainless steel molds sold for such purposes. I am using stainless steel large mixing bowls for a type of sand casting. I fire the mold up to 1500 and sometimes even to 1700 in order to melt the glass that is deeper in the sand. The molds themselves are mainly to contain the sand, not the glass. Judging by its looks, I will get another 4-5 fires before they are history. I will just have to sand them before each use to reduce the metal flakes.
As for now, I am firing organic looking pieces from glass beads for a series called "Primordial Life". Actually, sometimes the metal flakes make the piece look even more interesting. I will post these and others in the next 30 days as I get the new site up.
Thanks
Mike Hawkins
(still playing with glass)
			
			
									
						
										
						Anyway, I am sure these are not the quality stainless steel molds sold for such purposes. I am using stainless steel large mixing bowls for a type of sand casting. I fire the mold up to 1500 and sometimes even to 1700 in order to melt the glass that is deeper in the sand. The molds themselves are mainly to contain the sand, not the glass. Judging by its looks, I will get another 4-5 fires before they are history. I will just have to sand them before each use to reduce the metal flakes.
As for now, I am firing organic looking pieces from glass beads for a series called "Primordial Life". Actually, sometimes the metal flakes make the piece look even more interesting. I will post these and others in the next 30 days as I get the new site up.
Thanks
Mike Hawkins
(still playing with glass)
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
At 1700, I'm surprised you have any mold left. Stainless melts somewhere around 1800 or 1900, so I'm sure it's gotten pretty soft by the time you get to 1700.
I don't know anyone who uses their stainless steel molds at that high a temperature.
Tony
			
			
									
						
							I don't know anyone who uses their stainless steel molds at that high a temperature.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
SS melts at 2588F (1420C) What is the thickness of the steel?
This should be SS304 or possibly SS302 If the people you got it from don't know then don't deal w/ them again. If it is a scrap drop it could have been contamenated by someone grinding mild steel nearby and throwing slag on it. If you want to remove this problem, try an aggressive sandblasting and then soak a towel in vinegar, wrap the steel, put in a plastic bag overnight. The acid is a good way to remove millscale from mild steel; I've never seen this kind of thing in stainless (and I've had it in run-away kiln conditions). But that obviously doesn't mean it can't happen! 
 
Is it peeling inside and outside the mold?
			
			
									
						
							This should be SS304 or possibly SS302 If the people you got it from don't know then don't deal w/ them again. If it is a scrap drop it could have been contamenated by someone grinding mild steel nearby and throwing slag on it. If you want to remove this problem, try an aggressive sandblasting and then soak a towel in vinegar, wrap the steel, put in a plastic bag overnight. The acid is a good way to remove millscale from mild steel; I've never seen this kind of thing in stainless (and I've had it in run-away kiln conditions). But that obviously doesn't mean it can't happen!
 
 Is it peeling inside and outside the mold?
j.
A lack of doubt doesn't lend certainty.
			
						A lack of doubt doesn't lend certainty.
Yes, it is peeling on both sides.  The stainless steel molds are bowls from a department store. They had the name ssteal on the label. They are rather thin mixing bowls that I have used to slump glass over for drapes. Since then I just use them to contain my sand and do not allow the glass to touch the edges. When is peels, is this the same thing as spall? 
Anyway, thanks for the advice. I will just get a more professional version when these are done.
			
			
									
						
										
						Anyway, thanks for the advice. I will just get a more professional version when these are done.
- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Boy, I have to stop trying to quote melting temperatures from memory... and I'm not old enough to be losing that!!!jerry flanary wrote:SS melts at 2588F (1420C) What is the thickness of the steel?
This should be SS304 or possibly SS302 If the people you got it from don't know then don't deal w/ them again. If it is a scrap drop it could have been contamenated by someone grinding mild steel nearby and throwing slag on it. If you want to remove this problem, try an aggressive sandblasting and then soak a towel in vinegar, wrap the steel, put in a plastic bag overnight. The acid is a good way to remove millscale from mild steel; I've never seen this kind of thing in stainless (and I've had it in run-away kiln conditions). But that obviously doesn't mean it can't happen!
Is it peeling inside and outside the mold?
Tony

The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				jerry flanary
- Posts: 158
- Joined: Tue Sep 09, 2003 11:11 pm
- Location: norfolk, va
Just use a "vague-ifier" like "around" or "at about" :p I only knew exact because I googled it. But I knew 17-1900 seemed low. Melting temps are fun to think about...
The one I really find interesting though is the sterling silver VS. fine silver: Sterling is 1475F Fine is 1761F Copper is 1984F But Sterling is made by adding a little Copper to the Fine Silver. I think it is so odd how those two interact and cause the Sterling to have such a low melting temp. Where is a drunken material science major to explain this kinda crap when you really want one? (No body gets to answer "Alfred", ok?)
			
			
									
						
							The one I really find interesting though is the sterling silver VS. fine silver: Sterling is 1475F Fine is 1761F Copper is 1984F But Sterling is made by adding a little Copper to the Fine Silver. I think it is so odd how those two interact and cause the Sterling to have such a low melting temp. Where is a drunken material science major to explain this kinda crap when you really want one? (No body gets to answer "Alfred", ok?)
j.
A lack of doubt doesn't lend certainty.
			
						A lack of doubt doesn't lend certainty.
- 
				Joanne Owsley
- Posts: 52
- Joined: Wed Apr 16, 2003 4:27 pm
- Location: Arlington, WA
- Contact:
[quote="jerry flanary"]Just use a "vague-ifier" like "around" or "at about" :p I only knew exact because I googled it. But I knew 17-1900 seemed low. Melting temps are fun to think about...
The one I really find interesting though is the sterling silver VS. fine silver: Sterling is 1475F Fine is 1761F Copper is 1984F But Sterling is made by adding a little Copper to the Fine Silver. I think it is so odd how those two interact and cause the Sterling to have such a low melting temp. Where is a drunken material science major to explain this kinda crap when you really want one? (No body gets to answer "Alfred", ok?)[/quote]
I think I remember learning in Chemistry class that a solution will have a lower boiling point than either of the elements from which it was made. Same principle, perhaps?
			
			
									
						
							The one I really find interesting though is the sterling silver VS. fine silver: Sterling is 1475F Fine is 1761F Copper is 1984F But Sterling is made by adding a little Copper to the Fine Silver. I think it is so odd how those two interact and cause the Sterling to have such a low melting temp. Where is a drunken material science major to explain this kinda crap when you really want one? (No body gets to answer "Alfred", ok?)[/quote]
I think I remember learning in Chemistry class that a solution will have a lower boiling point than either of the elements from which it was made. Same principle, perhaps?
~ Joanne
"What neglected medication made you think THAT was a good idea??"
- me, to myself
			
						"What neglected medication made you think THAT was a good idea??"