BE Reactive Color Chart?

Post by KellyG »

Did a search in archives, but couldn't find info there.

Does anyone have or know where I can get a complete list of all BE reactive colors. I have a partial list from a hi-fire class, but I've seen reactions to colors not listed on my chart.

BTW, just out of curiosity, do spectrum colors react like BE?

Tiredofsurprisesgirl.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Bullseye will give you a list, they've published it before. Brock
My memory is so good, I can't remember the last time I forgot something . . .
KellyG
Posts: 67
Joined: Sun Mar 09, 2003 11:12 pm
Location: Baton Rouge, LA
Contact:

Post by KellyG »

If it's the "Information courtesy of Mary Kay Nichie", I have that, but it's incomplete. There's no date on it, so I don't know if it's the most recent.

I'll contact BE tomorrow. Just hoping that a list had been published on the web somewhere.

Still curious about Spectrum color reactivity.

Thanks ...K
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

KAG wrote:If it's the "Information courtesy of Mary Kay Nichie", I have that, but it's incomplete. There's no date on it, so I don't know if it's the most recent.

I'll contact BE tomorrow. Just hoping that a list had been published on the web somewhere.

Still curious about Spectrum color reactivity.

Thanks ...K
All colored glass is subject to reactions based on the chemicals chosen by the manufacturer to achieve the specific color.

- Paul
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Probably not a complete list, but here's a start: http://www.warmglass.com/cgi-bin/wgarch ... read=73891
KellyG
Posts: 67
Joined: Sun Mar 09, 2003 11:12 pm
Location: Baton Rouge, LA
Contact:

Post by KellyG »

Thanks Brad, great link. I didn't search old archives. Apparently, there's a wealth of info there.

I'm gonna print this one

...Kelly
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Re: BE Reactive Color Chart?

Post by Barbara Muth »

KAG wrote:Did a search in archives, but couldn't find info there.

Does anyone have or know where I can get a complete list of all BE reactive colors. I have a partial list from a hi-fire class, but I've seen reactions to colors not listed on my chart.

BTW, just out of curiosity, do spectrum colors react like BE?

Tiredofsurprisesgirl.
The safest thing to do is test! You may find interesting ways to capitalize on the reactions.

Reactionmadgirl
Barbara
Check out the glass manufacturer's recommended firing schedules...