Hazy look after clear cap
Moderators: Brad Walker, Tony Smith
Hazy look after clear cap
This is my first attempt at fusing, have read books and have been checking out the Bulletin Board Forums. Made a picture frame using Sys 96 glass, it came out ok for my first try. But i thought it would look better capped with clear glass. Fused piece again but about 2/3rds of it came out hazy, the other 1/3rd was crystal clear. What did i do wrong? Any comments will be appericated.
			
			
									
						
										
						- 
				Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
how did you clean the glass? Some people have had problems with one type of glass cleaner over another. I do a distilled water rinse/wipe after I wash the glass just to get rid of any residue that might be left behind from the cleaner.
Tony
			
			
									
						
							Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun