Cold Cuts
Moderators: Brad Walker, Tony Smith
- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
Cold Cuts
Unless it hits minus twenty this winter I am done with my outdoor cutting trials. Results of my latest effort were done at five below, and still no discernible difference. Despite my bulky gloves and heavy coat I was still able to run the scores with no trouble. I even threw in some Bullseye 3445, one of the more stubborn glasses in my palette, and it was on it's best behavior. Brrr....
			
			
									
						
										
						- 
				Kim Bellis
 - Posts: 133
 - Joined: Sat Jun 14, 2003 9:48 pm
 - Location: Tampa, Florida
 - Contact:
 
Re: Cold Cuts
Well, this is amazing! No one who tried this had any problems, right?Tony Serviente wrote:Unless it hits minus twenty this winter I am done with my outdoor cutting trials. Results of my latest effort were done at five below, and still no discernible difference. Despite my bulky gloves and heavy coat I was still able to run the scores with no trouble. I even threw in some Bullseye 3445, one of the more stubborn glasses in my palette, and it was on it's best behavior. Brrr....
All I can say is I have noticed this phenomena several times during workshops in cold climates, and all the other parameters were the same, even to the tools used.
Brock
My memory is so good, I can't remember the last time I forgot something . . .
			
						- 
				Rick Wilton
 - Posts: 273
 - Joined: Sat Oct 25, 2003 8:18 pm
 - Location: Calgary, Canada
 - Contact:
 
Brock,
I don't know about BE or spectrum but the guys from my supplier of float won't cut 19mm 3/4" float when it is fresh off the truck and very cold out. Now the questions becomes whats "COLD OUT" well here in Calgary today it's about -30 degrees celsius which works out to about -21 F I believe. That's COLD to me. Some people refer to glass as a super cooled liquid is thats what it is at 70 degrees F that it is a Super Duper Cooled liquid at -21 F.
			
			
									
						
							I don't know about BE or spectrum but the guys from my supplier of float won't cut 19mm 3/4" float when it is fresh off the truck and very cold out. Now the questions becomes whats "COLD OUT" well here in Calgary today it's about -30 degrees celsius which works out to about -21 F I believe. That's COLD to me. Some people refer to glass as a super cooled liquid is thats what it is at 70 degrees F that it is a Super Duper Cooled liquid at -21 F.
Rick Wilton
			
						Yeah, but Bert's cutting float in Maine winters. I don't get it. BrockRick Wilton wrote:Brock,
I don't know about BE or spectrum but the guys from my supplier of float won't cut 19mm 3/4" float when it is fresh off the truck and very cold out. Now the questions becomes whats "COLD OUT" well here in Calgary today it's about -30 degrees celsius which works out to about -21 F I believe. That's COLD to me. Some people refer to glass as a super cooled liquid is thats what it is at 70 degrees F that it is a Super Duper Cooled liquid at -21 F.
My memory is so good, I can't remember the last time I forgot something . . .
			
						- 
				Mark Hughes
 - Posts: 49
 - Joined: Mon Mar 17, 2003 6:27 pm
 - Location: Omaha, Nebraska
 
- 
				Allan Gott
 - Posts: 19
 - Joined: Mon Mar 10, 2003 11:57 am
 - Location: Calgary
 - Contact:
 
Part of not wanting to cut thick sheet when it's "fresh off the truck and very cold out" is a handling concern Rick. Any condensation plus the use of suction cups AND large, heavy sheets of thick float has the potential of making a huge and dangerous mess. 
If you can get it to the cutting table though, temperature was never a concern at any of the glaziers I worked for in the 1980's.
			
			
									
						
										
						If you can get it to the cutting table though, temperature was never a concern at any of the glaziers I worked for in the 1980's.
- 
				Rick Wilton
 - Posts: 273
 - Joined: Sat Oct 25, 2003 8:18 pm
 - Location: Calgary, Canada
 - Contact:
 
It never occured to me that condensation may be the problem, That may be what they were refering to but I'm sure I've heard it more than once that cutting cold glass was temperamental,  especially 12-19 mil. Maybe I misunderstood or maybe the guys were full of BS. Those who can't cut 19 mil well are always looking for an excuse. That's why there is only a few shops that will cut it. My new shop is only two blocks from the PPG warehouse and they won't touch the stuff locally. (Two bays down from  Fairbairn and Norton's you know them) If you want it you'll take a full sheet or nothing. It took me a while to figure out the art of cutting it well, I spent alot of time at a couple of local shops having them show me how they do it. Where did you work in the 80's ?
http://www.wiltonstudios.com
			
			
									
						
							http://www.wiltonstudios.com
Rick Wilton
			
						- 
				Allan Gott
 - Posts: 19
 - Joined: Mon Mar 10, 2003 11:57 am
 - Location: Calgary
 - Contact:
 
Late 70's/early 80's Rick at Western Aluminum and Commercial Aluminim. Didn't do a huge amount of thick cutting.  Enough to say I can do it, but we were hackers. We had to "trim" a dozen 1" entry doors one time - no pressure there. 
There used to be a distributor/supplier on the corner of Barlow and 70th(?). One day I was there picking up sealed units, a whole lowrider trailer loaded with thick float "exploded" in the indoor loading bay. Luckily it was still tarped but it took them a week to clean it up.
Yeah I know the Double Struggle boys. Good guys.
			
			
									
						
										
						There used to be a distributor/supplier on the corner of Barlow and 70th(?). One day I was there picking up sealed units, a whole lowrider trailer loaded with thick float "exploded" in the indoor loading bay. Luckily it was still tarped but it took them a week to clean it up.