I'm waiting to receive my Tauras 3 ring saw, which I have no experience using, and am wondering if I have to be really careful as to if it cuts through skin! No, really!!! I have had a home-made manicure using my grinder by accident, so I'm just wondering if this thing can buzz through my finger. Brock, I await your answer!!!!!!!!
Your friend,
Vickie
will I lose a finger!
Moderator: Brad Walker
I don't have one of those, I'm a fan of the tile saws. But I don't think your finger is in danger. Diamond blades and wire saws "grind" through glass, and you can actually touch the blade while it's running and not cut yourself. But don't!
My memory is so good, I can't remember the last time I forgot something . . .
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
What Brock said EXCEPT it WILL cut your fingernail. It likes hard thingsBrock wrote:I don't have one of those, I'm a fan of the tile saws. But I don't think your finger is in danger. Diamond blades and wire saws "grind" through glass, and you can actually touch the blade while it's running and not cut yourself. But don't!
Jim
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact: