Float glass devitrification spray or other technique
Moderator: Brad Walker
-
- Posts: 2
- Joined: Tue Jan 27, 2004 8:25 pm
Float glass devitrification spray or other technique
Anyone have technique for avoiding devit on float glass at 1600f?
-
- Posts: 1
- Joined: Mon Jul 21, 2003 8:27 am
- Location: Gloucester, On. Canada
Re: Float glass devitrification spray or other technique
Felt Glass wrote:Anyone have technique for avoiding devit on float glas
s at 1600f?
I use 'Clear Coat Overglaze" which is ideal for clear window
glass or plate
OR
Super Spray. Both these Fuse Master products come from Gil Reynolds
Fusion Headquarters. I consider both to be never-fails.
p.s.
Usually, I spray these products on.
neb