clear BE irid... qestion
Hi there - sorry to bother you guys but I've searched for this in the archives and apparently  I'm the only person who has a hard time telling the irid side on clear BE irid glass. When I was at Corning last year it was described as the "side that had a bit of a drag" indicating the metallic coating - but I've heard it described as the "rougher" side too. I am not getting it and some recent work is inconsistant due to this problem. Can you share any observations with me - besides disbelief? Ha - thanks - Lauralei
			
			
									
						
							Lauralei
			
						- 
				Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
- 
				Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Take a shape pencil and put the point on the surface of the glass. If the refection of the pencil touches the tip that is the irid side, if there is a space then that is the non-irid side. Do it once then feel the difference sides and you will suddenly see the difference. Thank you Brock. 
Rob
			
			
									
						
							Rob
"Come to the edge. We might fall. Come to the edge. It's too high! Come to the edge! And they came, and he pushed...... and they flew."
-- Christopher Logue
			
						-- Christopher Logue
- 
				daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR