Hi.
We are all affected by the entry of cheap Chinese products.
I'm a Filipino Chinese. Grew up in Philippines and our company has to compete with cheap China products in all product lines. Stained glass, sand relief casting, shower doors, wardrobe doors, glass sink.
Tried a dozen approach to compete. The best solution we found out is to build your reputation. Your reputation becomes a "brand". Brand for quality brand for expensive "worth it" products. After sales service.
Focus on the high end market. China products are focused on mass produced items. High end market always wants to have a unique value added product.
Ready made art glass doors are flooding the market, and every year we see them close up shop. Client participation in the design stage is very important. Particiaption makes the client feel they made the art glass.
my two cents
Nelson
Gecko fusible
Moderators: Brad Walker, Tony Smith
-
Nelson Tan
- Posts: 41
- Joined: Sun Mar 09, 2003 9:23 pm
- Location: Manila
- Contact:
-
daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR
-
Wallace Venable
- Posts: 38
- Joined: Sun Mar 09, 2003 8:34 pm
- Location: Morgantown, WEST Virginia
- Contact:
There have been several discussions of various forms of "fused batch" and/or "cullet" made specifically for re-melting in the studio. Some of this is/was coming from China, and early buyers were getting product not really ready for market.
Personally, at present I will stay away from this product, not because it's Chineese, but because of the "another COE to sort" and the "not certified by a proven vendor" issues.
I admire how much the Chineese glass producers have advanced in the past decade. Even the "dollar store" stuff gets better by the month.
Personally, at present I will stay away from this product, not because it's Chineese, but because of the "another COE to sort" and the "not certified by a proven vendor" issues.
I admire how much the Chineese glass producers have advanced in the past decade. Even the "dollar store" stuff gets better by the month.
Wally Venable, Student of glass
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada