I have a couple pieces with a burr on the edge -- a little sharp bit that's very unappealing. Small enough that it seems a waste to grind and go through a whole fire-polishing cycle ... is this something that a diamond hand pad would clean up?
Thanks -- Marilyn
use of diamond hand pad
Moderators: Brad Walker, Tony Smith
-
Marilyn Kaminski
- Posts: 22
- Joined: Wed Mar 12, 2003 10:27 am
- Location: Boulder, CO
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
The diamond pads will work, but I find them hard to control on small edges. One slip and you scratch the surface of your piece.
For fine details I like to use diamond honing sticks.
http://shop.woodcraft.com/Woodcraft/pro ... D4637914AA
Ron
For fine details I like to use diamond honing sticks.
http://shop.woodcraft.com/Woodcraft/pro ... D4637914AA
Ron
-