Post by Wayne »

I was just wondering if anyone has used this and if so have any recommendations as the best way to apply and or fire it.

Thanks!
_-_-_-_-_-_-_-_-_-_-_-_-_-_-_-_-

Wayne
WM Glass Studios
Image
Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

check the archives

Post by Cheryl »

lots of info on this in the archives. in sum: most people were underwhelmed with the results.
Stuart Clayman
Posts: 224
Joined: Mon Mar 31, 2003 12:35 pm
Location: Virginia
Contact:

Post by Stuart Clayman »

I even contacted the manufacturer and one of the women that I talked to suggested that I use a spray enamel on the back and don't use their product.

Stuart
Wayne
Posts: 5
Joined: Wed Dec 03, 2003 5:26 pm
Location: Utah
Contact:

Post by Wayne »

Thanks Cheryl and Stuart.
_-_-_-_-_-_-_-_-_-_-_-_-_-_-_-_-

Wayne
WM Glass Studios
Image
Post Reply