flat lap questions

Post by Paul Tarlow »

Where to buy?

What to look for?

In the words of Hans Schultz,


"I know nothing..."
Last edited by Paul Tarlow on Fri Feb 06, 2004 9:52 am, edited 1 time in total.
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Re: flat lap questions

Post by Brian and Jenny Blanthorn »

Paul Tarlow wrote:Where to buy?

What to look for?

In the words of Hans Schultz,


"I know nothing..."
What size ??

His glass has a plan of one U build ur self

U can also buy second hand ones

Brian
Image
Mark Hughes
Posts: 49
Joined: Mon Mar 17, 2003 6:27 pm
Location: Omaha, Nebraska

Post by Mark Hughes »

Try SW Diamond Products, 1-800 825-2792 , PO Box 116, Gorman, Ca 93243 . They were at Glass Craft Expo last year.
Mark Hughes
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

I am a fan of SW. I have his 24" magnetic lap, going on 13 years old. Only maintenance has been a new belt for $8.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Thanks all for responding. I took a look at SW's site -- which only exposed additional ignorance on my part :)

I my primary use will be bowl edges. What grits are people using? Also, can someone enlighten me to the benefits of a plain vs grooved disk?

Mucho gracias

- Paul
Susan Moore
Posts: 96
Joined: Mon Oct 06, 2003 10:07 pm
Location: Austin, TX
Contact:

Post by Susan Moore »

What is SW's website please. Mucho, mucho gracias!

Susan
charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Post by charlie holden »

In case Brian's post seemed a little cryptic, try: http://www.hisglassworks.com

He sells all kinds of abrasives stuff, has lots of helpful advice online and gives great phone help.

ch
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

I didn't know he was still selling ungrooved. What happened to my first 24" pad, ungrooved, was after five years or so of daily use, it became a big, magnetic, diamond plated taco. I think the daily compression on the center third or so of the pad deformed it and caused the warp. The idea behind the grooves is similar to expansion joints in concrete, it allows a certain amount of expansion without affecting the integrity of the whole. The grooved pad is going strong with no tendency toward mexican food.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Susan Moore wrote:What is SW's website please. Mucho, mucho gracias!

Susan
http://swdiamond.freeyellow.com

Be warned -- they use a fee internet host that pops up all kinds of ads and more. It will probably asky you if you want to install this thing or that thing. Answer NO every time. I can swear to it but I'd bet my house that some of it was spyware.

My bet is they've lost a lot more business based on the freeyellow (the host) junk than they've savded. Just imo.

- Paul
scooter riegelsperger
Posts: 26
Joined: Fri Mar 14, 2003 9:23 am
Location: Houston,TX
Contact:

Post by scooter riegelsperger »

The primary reason of grooves or ripples in face of disc is to hold coolant.
They also provide for faster removal of stock. The finer the grit the less reason for grooves. If you're going to be just doing edges & bevels,I would reccomend no grooves. Crystalite is a good source for discs and grinders.
Do illiterate people get the full effect of alphabet soup?
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Paul Tarlow wrote:Thanks all for responding. I took a look at SW's site -- which only exposed additional ignorance on my part :)

I my primary use will be bowl edges. What grits are people using? Also, can someone enlighten me to the benefits of a plain vs grooved disk?

Mucho gracias

- Paul
60, 140, 220, wet belt (220) on the edge, sandblast w/180 SiCa.

No grooves.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

what's the life span of a good quality diamond disk

they are very spendy
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

I find BE to be really hard on the disks, but I'm removing a lot of material all the time. If you're just flattening the bottoms of things, especially clear batch or cullet blown stuff, you can expect years out of a plate. I buy a new 60 grit plate every 4 or 5 months.
If you need the technology for your work you've got to include its cost in the price.
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Post by Brian and Jenny Blanthorn »

Paul Tarlow wrote:Thanks all for responding. I took a look at SW's site -- which only exposed additional ignorance on my part :)

I my primary use will be bowl edges. What grits are people using? Also, can someone enlighten me to the benefits of a plain vs grooved disk?

Mucho gracias

- Paul
U thinking of diomond or loose grit ??

Brian
Image
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Brian and Jenny Blanthorn wrote:
Paul Tarlow wrote:Thanks all for responding. I took a look at SW's site -- which only exposed additional ignorance on my part :)

I my primary use will be bowl edges. What grits are people using? Also, can someone enlighten me to the benefits of a plain vs grooved disk?

Mucho gracias

- Paul
U thinking of diomond or loose grit ??

Brian
I'd like to hear pros and cons of each -- never having heard either.

- Paul
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Post by Brian and Jenny Blanthorn »

Paul Tarlow wrote:
Brian and Jenny Blanthorn wrote:
Paul Tarlow wrote:Thanks all for responding. I took a look at SW's site -- which only exposed additional ignorance on my part :)

I my primary use will be bowl edges. What grits are people using? Also, can someone enlighten me to the benefits of a plain vs grooved disk?

Mucho gracias

- Paul
U thinking of diomond or loose grit ??

Brian
I use loose grit on 36 " wheel

60 + old stuff

Then strait on2 rociprolap

Brian

I'd like to hear pros and cons of each -- never having heard either.

- Paul
Image
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Post by Kevin Midgley »

Bowl edges? Flat lap? Why not a belt sander? I would never use the SW machine I once had to do bowl edges, for the Bee belt sander was so much more forgiving. If you want flat bottoms on warped bowls or vases made of Baroque which has uneven thickness, then the lap is the way to go. Brian's system is essentially a table that shakes rattles and rolls for a period of time with the glass item to be flattened allowed to grind away a surface area. From my understanding of the lapidary processes Brian uses, I do not think he would or could use his system to do the edges on a bowl.
SW machines have a center water feed and you can use the entire surface of a disk. Some machines have a central lock down post which would cut the usable disk area in half since you would not want to hit the post! Some machines have a water feed tube which drips onto the grinding disk. The water is not in that system fed as directly to the surface of the disk as an SW machine and the water feed tube can get in the way when you are grinding. Some machines will operate not using diamond disks and water feed. Instead they use a slurry of water and carbide or diamond dripped onto a steel wheel. In that system if you are trying for a polish and contaminate a fine grit with a coarse grit you will have to start your polishing over.
The SW machine I had started to develop bearing problems. I recently enquired of Steve at SW via email as to the approximate cost etc. of replacing that area of a new machine I might buy but did not get a reply to that question. Mine was an older model and perhaps the squeeky bearing problems have been resolved with later versions. the SW design was good enough that the workers at Corning liked the machines. If I was to buy a lap I would probably go with an SW despite the failure to get an answer to my question.
I never got good at polishing on it for I did not like to spend the time and I did not know about the different types/grades of cerium oxide. Beware the fact I read somewhere about cerium often being trace contaminated with thorium??? Don't want to breathe it or eat it.
Final words for an SW lap user....hold onto your glass REALLY well and as you are standing there using the lap, ask yourself why you didn't make the area you are grinding, flat in the first place so that you wouldn't have to be standing there using the machine.
Kevin in Tofino with budding daffodils.
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Post by Brian and Jenny Blanthorn »

Kevin Midgley wrote:Bowl edges? Flat lap? Why not a belt sander? I would never use the SW machine I once had to do bowl edges, for the Bee belt sander was so much more forgiving. If you want flat bottoms on warped bowls or vases made of Baroque which has uneven thickness, then the lap is the way to go. Brian's system is essentially a table that shakes rattles and rolls for a period of time with the glass item to be flattened allowed to grind away a surface area. From my understanding of the lapidary processes Brian uses, I do not think he would or could use his system to do the edges on a bowl.
SW machines have a center water feed and you can use the entire surface of a disk. Some machines have a central lock down post which would cut the usable disk area in half since you would not want to hit the post! Some machines have a water feed tube which drips onto the grinding disk. The water is not in that system fed as directly to the surface of the disk as an SW machine and the water feed tube can get in the way when you are grinding. Some machines will operate not using diamond disks and water feed. Instead they use a slurry of water and carbide or diamond dripped onto a steel wheel. In that system if you are trying for a polish and contaminate a fine grit with a coarse grit you will have to start your polishing over.
The SW machine I had started to develop bearing problems. I recently enquired of Steve at SW via email as to the approximate cost etc. of replacing that area of a new machine I might buy but did not get a reply to that question. Mine was an older model and perhaps the squeeky bearing problems have been resolved with later versions. the SW design was good enough that the workers at Corning liked the machines. If I was to buy a lap I would probably go with an SW despite the failure to get an answer to my question.
I never got good at polishing on it for I did not like to spend the time and I did not know about the different types/grades of cerium oxide. Beware the fact I read somewhere about cerium often being trace contaminated with thorium??? Don't want to breathe it or eat it.
Final words for an SW lap user....hold onto your glass REALLY well and as you are standing there using the lap, ask yourself why you didn't make the area you are grinding, flat in the first place so that you wouldn't have to be standing there using the machine.
Kevin in Tofino with budding daffodils.
I can do a flat edge on a bowl

If I wana do a rounded edge I would use linisher

Diomond goes a lot faster than grit

But using different pullies n magnetic diomond U could use either

I flat my flat bed off with car wheel hub

Brian
Image
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Post by Paul Tarlow »

Okay - still looking for a solution for bowl edges.

I looked at the flat lap plans on hisglassworks.com -- it is straight forward enough but I'm not sure where to get the 23.5" x 0.5" steel circle.

I'd also like to hear who has experience with one of these:

http://www.hisglassworks.com/pages/air658.html

and what your thoughts are.

Thanks,
Paul
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

Just curious what type of bowl edges you're after Paul. I don't remember if you have a wbs of not?

If you're after an edge like this bowl you need the flat lap grinder. I call this one a flat grind, very time consuming if you polish it to a mirror finish. It takes more than an hour of hard work to get this type of edge.

Image

If you're after the bevel ground edge like this one, only the wbs will do.

Image

The bevel grind is quick and takes less than maybe 15 minutes.

Both ground rim types are somewhat more fragile than a plain fused rim.

Ron