I've searched the archives and couldn't find an answer. Is Primo kiln wash suitable for high firing, e.g. 1700F for combing?

Cheers,
Suzan
carol nahoom
Posts: 17
Joined: Mon Nov 03, 2003 8:12 am
Location: Crawfordville, Florida

primo primer

Post by carol nahoom »

Hi Suzan -

"Primo is designed for fusers who fire on the high end of the fusing range, specifically 1500-1550 instead of the usual 1425-1475". This is what the brochure says that I got with my primo. Combing would definitely be at the high end of the fusing range. Hope this helps. Carol
Bryan
Posts: 26
Joined: Wed Jan 07, 2004 4:42 pm
Location: Houston,TX

Post by Bryan »

Suzan

Have you found any kiln wash for high firings?
( 1700F )
If so please let me know?
Thanks
BZody
Suzan
Posts: 75
Joined: Mon Mar 17, 2003 12:22 pm
Location: Ottawa, Ontario Canada
Contact:

Post by Suzan »

Bryan-Zody

I've been using Bullseye kiln wash and it works fine for combing. It does stick to the glass after a combing, but comes off with vigourous scrubbing. If there are trace amounts of kiln wash left, I use "Velvet Etch"
etching creme to remove it.

I recently switched to Primo because I absolutely hate scraping shelves, and Primo rubs off easily. I was concerned that, because it does rub off so easily after fusing, that it might not act as a good separator for high-range firing, i.e. over 1650F.

I wasn't able to find a website for Hotline, anyone know it?

Cheers,
Suzan
Cynthia

Post by Cynthia »

Bryan-Zody wrote:Suzan

Have you found any kiln wash for high firings?
( 1700F )
If so please let me know?
Thanks
BZody
Hotline makes a kiln wash for high temp firing called appropriately enough, "HI-FIRE" Shelf Primer. Wherever you are getting your Primo from should sell this too.
Kim Bellis
Posts: 133
Joined: Sat Jun 14, 2003 9:48 pm
Location: Tampa, Florida
Contact:

Post by Kim Bellis »

Suzan wrote:I wasn't able to find a website for Hotline, anyone know it?
Susan:
I believe this is the site your looking forhttp://www.fusionheadquarters.com/

Kim
dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Post by dee »

Bryan-Zody wrote:Suzan

Have you found any kiln wash for high firings?
( 1700F )
If so please let me know?
Thanks
BZody
the hotline hi-fire flavor of kilnwash works well, also soaking in vinegar removes kilnwash afterwards.....
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Lynne Chappell
Posts: 186
Joined: Fri Mar 14, 2003 2:05 am
Location: Surrey B.C. Canada
Contact:

Post by Lynne Chappell »

I believe Hotline is Ed Hoy's (Creative Craftsmen) brand name.

I haven't used the Primo yet. Is there the same kind of health hazards with the dust as with thinfire? I wouldn't think so, but then you never know.