large sink slump
Moderators: Brad Walker, Tony Smith
large sink slump
Before making my first attempt to slump a 3/4 inch thick 18 inch diameter blank thru a drop ring....I feel the need for group support
Okay, I set up six 1" square poles (furniture) to hold the drop ring. Will this hold the weight of the glass? or is there a better set-up for this large heavy blank. The poles are 9inches high because I want to get a deep drop. I will wait for all you professionals out there before firing because I would hate for all this glass to tble over in my kiln.
What would I do without all of you
Thanks in advance........
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Doc
A 9" slump is asking for disaster. Keep it to 5" and enjoy success. The deeper you go, the bigger the chance it ill fall in.
A 9" slump is asking for disaster. Keep it to 5" and enjoy success. The deeper you go, the bigger the chance it ill fall in.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Barbara Cashman
- Posts: 151
- Joined: Sun Mar 09, 2003 5:42 pm
- Location: Greensboro NC
- Contact:
Bert's exactly right. I go for a 4 1/2 to 5" drop. You'll keep the thickness at the lowest point at about 1/2". I wouldn't suggest anything thinner. If you set a kiln-washed shelf under the drop, you can stop the drop with a slight flat spot for drilling the hole. Also, as said before, check your setup with a level before firing. - Barbara