Can somebody give me an accurate weight on a 2" x 4" piece of glass in standard thickness (3mm) and thin (1.6mm). I've been tracking the sales of scrap glass on the Internet. Most of the glass is sold by weight- usually in 1/4 lb or 1lb increments but I have seen it sold by the ounce. Just curious to find out just how good of a "deal" they are.
Steve
Glass Weight
Moderators: Brad Walker, Tony Smith
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Glass weighs 155 lbs/ft³ or 0.0897 lbs/in³. So a 2 x 4 x 3mm (0.118") piece of glass is 0.944 in³ x 0.0897 lbs/in³ = 0.0847 lbs or a little less than 1/10 of a pound. 1.6 mm thickness is just about half that or 0.504 in³ which gives you 0.045 lbs or 1/22 of a pound.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Goldfinger
- Posts: 54
- Joined: Wed Jan 07, 2004 11:07 am
- Location: Missouri
Glass Weight
Wow- I didn't think we had any mathematicians on board. It was a big help.
Thanks Tony
Steve
Thanks Tony
Steve