Fusing float glass with Spectrum 96??
Moderators: Brad Walker, Tony Smith
Fusing float glass with Spectrum 96??
I'm soooo new to this and doing lots of experimenting. Just tried some 96 stingers and frit on float glass and it seems to be a success. Will it perhaps break later? 
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
It could break tonight, or it could break next year... but float and 96 are not compatible and you will eventually start seeing cracks or crazing along the edges of the 96 glass.