Hi I am looking for a conversion chart to convert copper foil gauge to mil. Nimrod Hall sells by mil, I have some copper that is 40 ga. I am at a loss as to how to find my answer. I read the archives no help, so did a search on the internet nothing. I thought this would be a simple thing to find. Thanks, Nanc
-
Larry Lunsford
- Posts: 38
- Joined: Thu May 08, 2003 4:26 pm
- Location: Littleton, CO
- Contact:
Here's a conversion from gauge to inches:
Gauge Inches
000 0.41
00 0.365
0 0.325
1 0.289
2 0.258
3 0.229
4 0.204
5 0.182
6 0.162
7 0.144
8 0.128
9 0.114
10 0.102
11 0.091
12 0.081
13 0.072
14 0.064
15 0.057
16 0.051
17 0.045
18 0.04
19 0.036
20 0.032
21 0.0285
22 0.0253
23 0.0226
24 0.0201
25 0.0179
26 0.0159
27 0.0142
28 0.0126
29 0.0113
30 0.01
31 0.0089
32 0.008
33 0.0071
34 0.0063
35 0.0056
36 0.005
37 0.0045
38 0.004
39 0.0035
40 0.0031
Gauge Inches
000 0.41
00 0.365
0 0.325
1 0.289
2 0.258
3 0.229
4 0.204
5 0.182
6 0.162
7 0.144
8 0.128
9 0.114
10 0.102
11 0.091
12 0.081
13 0.072
14 0.064
15 0.057
16 0.051
17 0.045
18 0.04
19 0.036
20 0.032
21 0.0285
22 0.0253
23 0.0226
24 0.0201
25 0.0179
26 0.0159
27 0.0142
28 0.0126
29 0.0113
30 0.01
31 0.0089
32 0.008
33 0.0071
34 0.0063
35 0.0056
36 0.005
37 0.0045
38 0.004
39 0.0035
40 0.0031
-