Hello everyone, I want to make my own molds. Can anyone give me a great recipe to make a mold that will do well and I can reuse in my firings for fusing glass?
I have heard a lot about hydrocal,silcia,etc. If there are anyone that can and will share a good recipe with me I would be most appreciative. In addition to anything regarding some sculpture.
I have read some books,
I want someone that has experienced the results.
Thanks in advance for any comments, suggestions.
Mold Making Recipe
Moderators: Brad Walker, Tony Smith
-
whitejoyce
- Posts: 28
- Joined: Sat May 10, 2003 6:06 pm
- Location: Phoenix,AZ
Mold Making Recipe
Last edited by whitejoyce on Thu Feb 19, 2004 6:14 pm, edited 1 time in total.
J. White
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Depends on what type of mold you need. Plaster and silica are only good for one trip in the kiln and then they fall apart. They do make good molds but are used mainly for casting glass.
For a reusable mold try something like raku clay from a pottery supply store.
You can form the clay, dry it, and then fire it in your kiln.
Lots in the archives and a few current threads about making molds.
Ron
For a reusable mold try something like raku clay from a pottery supply store.
You can form the clay, dry it, and then fire it in your kiln.
Lots in the archives and a few current threads about making molds.