Regular float glass is safe to eat off. The crystal clear and tinted floats are also good. I don't know about lowE...
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Sandwiching is tricky. My technique is to prefire the enamels. I recently heard about a technique of mixing the enamel with methyl cellulose medium (Klyr Fire) and not prefiring. I haven't tried this yet, myself.GatorGirl wrote:Thanks Bert. I thought so. I e-mailed Ferro about sandwiching some of their food safe enamels between float glass and the man I e-mailed panicked! He panicked so I panicked.
When you talk to Ferro, you might be interested in their china paints as well as glass enamels. In Germany you can get the transparent glass colors that are not available to us in the USA. They might work very well sandwiched. Different colors will behave differently. They are probably lead bearing, but once they are sandwiched, there are no more problems. I wish we could get these colors. They are fabulous looking. Be sure to put both air sides of the float glass in contact with the enamels. I would not fire hotter than 1420ºF to fuse the layers together. Soak for an hour somewhere around 1100 - 1220ºF on the ramp up.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Thanks Bert for all of the info. Do you know why they don´t sell the transparents to the US? I plan on visiting Frankfurt in a few weeks I guess I could ask them then. I guess that is where their main headquarters are. (By the way I loved your table top that you made by sand casting... using a jar lid for the texture!)