I was wondering if anyone ever slumped glass with cellular concrete. I have seen this product In France and the use it ti insulate the houses but it is porous like refractory bricks so I was wondering how it handle itself with the heat...
cellular concrete
Moderators: Brad Walker, Tony Smith
-
east-coast-jacques
- Posts: 4
- Joined: Fri Feb 13, 2004 10:36 am
- Location: Caraquet, NB, Canada
- Contact:
cellular concrete
good day all from the snow and cold of east coast Canada.
I was wondering if anyone ever slumped glass with cellular concrete. I have seen this product In France and the use it ti insulate the houses but it is porous like refractory bricks so I was wondering how it handle itself with the heat...
I was wondering if anyone ever slumped glass with cellular concrete. I have seen this product In France and the use it ti insulate the houses but it is porous like refractory bricks so I was wondering how it handle itself with the heat...
There is a fine line between a hobby and loosing your mind...
Jacques
Jacques
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
-
Stuart Clayman
- Posts: 224
- Joined: Mon Mar 31, 2003 12:35 pm
- Location: Virginia
- Contact:
I was at the ACC show today in Baltimore. I saw an artist there that had fused pieces of glass inside concrete/cement (don't know what it was) and then cold worked it to a high polish. Nice stuff, unfortunately the artist was not in the booth, just a helper that did not know the process.
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: cellular concrete
If its the stuff I think it is its very softeast-coast-jacques wrote:good day all from the snow and cold of east coast Canada.
I was wondering if anyone ever slumped glass with cellular concrete. I have seen this product In France and the use it ti insulate the houses but it is porous like refractory bricks so I was wondering how it handle itself with the heat...
I not used it but here R some thoughts
As its got air in dont fast fire possibilyty of small explosion
Fire dry
Fire small test peice
Brian

Across the road from my cafe is a sculptor who uses 'Hebel Bricks' which her husband is the local building supplier of such product.
I haven't had time to test it for possible use, but am told that it insulates, handles great heat but degrades to a powdery surface on the side that cops the heat.
It is light weight, porous and easy to shape which is obviously the pros.
regards, haydo
I haven't had time to test it for possible use, but am told that it insulates, handles great heat but degrades to a powdery surface on the side that cops the heat.
It is light weight, porous and easy to shape which is obviously the pros.
regards, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!