I dumpster dove a nice piece of 1/4" float.
Cut out 1/8" fiber paper pine trees ect.
spritzed on some borax and slumped.
500 dph to 1200 hold 20min
afap to 1450 hold 20 min then annealed
when I opened the kiln it was perfect..sorta
It was crystal clear!!! where is the beautiful pale green
I associate with fused float?? now I guess I will sandbalst
the front and slump for the matte finish Drat!
I want that pretty pale green color