			Is it normal for kiln bricks to crack, nothing large, just small fissures that run for a few inches?
			
			
									
						
										
						 
		 
				
		
		 
	 
				
		
		
			- 
				
																			 Brock
- Posts: 1519
- Joined: Mon Mar 10, 2003 1:32 pm
- Location: Vancouver, B.C.
						
					
						
		
													
							
						
									
						Post
					
								by Brock » 
			
			
			
			
			Yup. Brock
			
			
									
						