Some of my dichro pendants would look better with a gold bail. I've tried 14 K gold wire between layers, it held up for the firing (unlike sterling silver wire) but became so black I can't seem to get it clean. A local jewler suggested a higher 22 K gold. Has anyone tried that?
 Another suggestion was to get silver or nickle plated gold. Locally there is onle a place that does not specialize in jewlery with a $45.00 minimum and no over the phone quote.
 I haven't tried brass or bronze, how do they fire? Just the look of gold would be fine with me. I have a great little book about patina's but can't find it at the moment. Any suggestions?
http://community.webshots.com/user/lynfeu
			
			
									
						
										
						gold wire for pendants?
Moderators: Brad Walker, Tony Smith
- 
				Cheryl Wade
- Posts: 26
- Joined: Sun Mar 23, 2003 5:48 pm
- Location: Wales UK
Lyn
There's a site which may have something suitable - http://www.wire-scuplture.com which sells a vast range of precious and base metal wire. They're in MS, sorry, I don't know what state this is the abreviation for. I was looking for a UK supplier of silver wire to include when fusing and found this, so I'll be ordering some soon. What guage would you recommend for pendants?
Cheryl
			
			
									
						
										
						There's a site which may have something suitable - http://www.wire-scuplture.com which sells a vast range of precious and base metal wire. They're in MS, sorry, I don't know what state this is the abreviation for. I was looking for a UK supplier of silver wire to include when fusing and found this, so I'll be ordering some soon. What guage would you recommend for pendants?
Cheryl
- 
				Geri Comstock
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
There's a typo in the name which is why it wouldn't display for you.
Try this link:
http://www.wire-sculpture.com
Geri
			
			
									
						
										
						Try this link:
http://www.wire-sculpture.com
Geri
- 
				Cheryl Wade
- Posts: 26
- Joined: Sun Mar 23, 2003 5:48 pm
- Location: Wales UK
- 
				Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact: