Fastest way to make holes

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
jer99
Posts: 4
Joined: Tue Dec 13, 2011 4:56 pm

Fastest way to make holes

Post by jer99 »

I have to create multiple holes (4-5h in multiple wine bottle tops
I know that the tried and true method of making holes would be to drill.

This may take quitea while and was wondering if there was a faster method. I was thinking of some sort of torch since the only equipment I have is a kiln. I don't think a kiln will be useful as it might deform the glass.

Any ideas out there?
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Fastest way to make holes

Post by jim burchett »

Drill baby drill
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Fastest way to make holes

Post by AndyT »

I can drill a hole in a wine bottle in less than a minute with a drill press and the bottle submerged in water in a big plastic tub.
Tod
Posts: 36
Joined: Tue Feb 14, 2006 5:47 pm
Location: Massachusetts

Re: Fastest way to make holes

Post by Tod »

I'm not sure exactly what you're doing, but abrasive water jet machines make sweet holes in glass. You do need to be going thru only one thickness. Holes of almost any size (& shape!) can be drilled this way.
If you're making a series around a ring, you or the operator will need to devise a way to index the workpiece. Not that hard to do, but can be costly. Good for multiples. - Tod
please visit Beall Glass Studio on Face Book
Jeff Wright
Posts: 23
Joined: Tue Jun 24, 2003 4:40 pm

Re: Fastest way to make holes

Post by Jeff Wright »

I just recently tried an experiment to drill holes via sandblasting. Had some blown vessels that were 5-6mm thick. I created a simple stencil with a paper punch. Then I just concentrated the sandblasting in one area. I found that I made some really nice holes that way. Of course, I had to protect the inside of the vessel with newspaper so that when I actually blasted through the glass, the inside of the vessel didn't get sandblasted too!
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Fastest way to make holes

Post by Brock »

A friend of mine uses his sandblaster to cut large sheets of 12mm float for room dividers and sculptures.
He clamps the sheet above and below the proposed cut line and just blasts through it.
But ya gotta have the horses . . .
Post Reply