Simple lay up gives depth
Moderator: Brad Walker
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Simple lay up gives depth
This simple lay up gives depth to this piece. There will always be space between the top and bottom layers. 
Love and luck make a wonderful lifestyle.
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: Simple lay up gives depth
The photo didn't post.
This simple lay up gives much depth to this piece. There will forever be a space between the top and bottom layers. The orange pieces will forever cast a shadow on the stringers below.
This simple lay up gives much depth to this piece. There will forever be a space between the top and bottom layers. The orange pieces will forever cast a shadow on the stringers below.
Love and luck make a wonderful lifestyle.
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Simple lay up gives depth
How 'bout a picture of the fired result?
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: Simple lay up gives depth
Fired results will be out of the kiln on Wed or Thur.
Love and luck make a wonderful lifestyle.
-
Dairy Queen
- Posts: 71
- Joined: Sat Jun 18, 2005 8:33 am
- Location: Charlotte, NC
- Contact:
Re: Simple lay up gives depth
Here is the piece after the first firing. There are some tiny bubbles... Should have used a chad.