boron nitride
I have a can of boron nitride and was wondering if you all like to use it on stainless steel or do you feel that kiln wash works better?
Karyn
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
Re: boron nitride
A properly prepared SS mold can last YEARS with KW . . .
-
Karyn Cott
- Posts: 13
- Joined: Wed Sep 28, 2005 4:19 am
- Location: Poulsbo, WA
Re: boron nitride
One other question. I am draping over a ss form for a lamp shade. I want somewhat of a texture to the inside so that the light from the bulb is diffused. Would it work if I draped fiber blanket (that I separate into a thinner piece) over the ss form?
Karyn
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
Re: boron nitride
It would be better to impart the texture to the shade in a hotter firing on a kiln shelf. Then slump.