Is dichro slide supposed to go under clear glass or fire hot? I put some on some rather bland pendants - on top. I only took it to fire polish - 1350. It looked funny to me as I was carefull applying it; it seemed some had come off the edges. I rubbed the top of one of the pieces and it came off on my hand. It didn't come with any directions; I did a search on here with no results. Anyone have any clues - I'd be grateful. Thanks.
Patty
Dichro Slide
Moderators: Brad Walker, Tony Smith
Dichro Slide
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Dichro Slide
you get what you pay for.
Re: Dichro Slide
I checked the Glasshopper website (www.glasshopperpatterns.com). Their dichro slide instructions say it works well uncapped, and they recommend using your "usual fusing" schedule. I suspect it needs to be fired up into the fusing range rather than just a firepolish.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell
Re: Dichro Slide
Thanks Lynn - I appreciate your helpfulness. Patty
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
Re: Dichro Slide
Most of the manufacturers have very helpful tech support people. If you don't know the manufacturer, call your supplier and find out.
Take care.
Dawn
Dawn
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Dichro Slide
Lynn's right. If you want to use it uncapped, you'll need to fire high enough to get the slide to melt a bit into the piece. A full fuse works best.
-
Raphael Schnepf
- Posts: 24
- Joined: Sat Oct 14, 2006 11:31 pm
- Location: Milwaukie Oregon
- Contact:
Re: Dichro Slide
My wife Margaret uses Dichroslide a lot and prefers the look under a thin layer of clear. She has sandwiched it between several layers. Just like dichro glass the look is different (brighter) under clear glass.
Raf
Raf
-
Raphael Schnepf
- Posts: 24
- Joined: Sat Oct 14, 2006 11:31 pm
- Location: Milwaukie Oregon
- Contact:
Re: Dichro Slide
By the way Kevin this stuff's not cheap. It has its uses and works in ways the would be impossible for dichro glass.you get what you pay for.
Raf