how to remove silicone glue?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

how to remove silicone glue?

Post by Nina Falk »

I used some silicone glue, it did the trick, and now I want to remove it, completely. Suggestions? It's been on the piece for about a month.
Nicole Hanna
Posts: 27
Joined: Wed Jul 27, 2005 10:17 am
Location: SW Missouri
Contact:

Re: how to remove silicone glue?

Post by Nicole Hanna »

Razor blade works if you can get it behind the glue. I think some chemical dissolves it but can't remember what it is....acetone? mineral spirits? My husband is gone and not answering his phone! :roll:

N.
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: how to remove silicone glue?

Post by Bert Weiss »

You want to get as much as possible off with the razor blade, and your thumb, then clean up the residue with acetone.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: how to remove silicone glue?

Post by Nina Falk »

can't wait. thanks.
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: how to remove silicone glue?

Post by Greg Rawls »

The only way I found to successfully remove silicone from glass is to put the glass in the kiln and take it to 800.
Greg
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: how to remove silicone glue?

Post by Brock »

There is a commercial Silicone solvent. Nasty stuff.
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: how to remove silicone glue?

Post by rosanna gusler »

mek works. also nasty. rosanna
artist, owner of wanchese art studio, marine finisher
Tod
Posts: 36
Joined: Tue Feb 14, 2006 5:47 pm
Location: Massachusetts

Re: how to remove silicone glue?

Post by Tod »

I have successfully used razor blades and thumb nails but find that I often want to make it pretty by using 0000 steel wool with some whiting. The whiting helps stop the silicone from re-sticking and the steel wool, as much as I don't like using it, is fairly gentle as it removes more & more silicone, with little more whiting and some elbow grease. - Tod
please visit Beall Glass Studio on Face Book
dawnsud
Posts: 42
Joined: Mon Aug 01, 2005 5:03 pm
Location: Cedaredge, Colorado

Re: how to remove silicone glue?

Post by dawnsud »

Paint thinner works on E6000. Might try it on silicone.
Take care.
Dawn
Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: how to remove silicone glue?

Post by Georgia Novak »

Many years ago when I first started stained glass, I glued a panel into the grooved out area of a wooden door, per instructions of teacher. Well, or course a piece broke and the panel had to be removed. I wrote to e-6000 and asked how. They sent me a list in order from weak to strong. I think I finally ended up using turpentine which was the strongest on the list. It took a while but finally gave. Sorry for the shaggy dog story. Georgia