Hi,
I just received my handy-dandy circle cutter but no instructions. I just scored a beautiful, even circle. Now what? How do I get the circle out of the glass. I've tried tapping. I cut a score into the circle line and broke some of the border off. Is this how it is done. Seems like I might break my circle that way. Help! Please.
Sharon
Cutting a Circle
Moderators: Brad Walker, Tony Smith
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Try the circle cutting tutorial on Patty Gray's website. http://www.pattygray.com. It's also on the Spectrum website.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Re: Cutting a Circle
After a few hundred circles, you will easily be able to do this... but, first try Patty's way for sake of your pocketbook.artisand wrote:Hi,
I just received my handy-dandy circle cutter but no instructions. I just scored a beautiful, even circle. Now what? How do I get the circle out of the glass. I've tried tapping. I cut a score into the circle line and broke some of the border off. Is this how it is done. Seems like I might break my circle that way. Help! Please.
Sharon
-
Debinsandiego
- Posts: 41
- Joined: Mon May 19, 2003 6:47 pm
When I'm cutting a circle in an opal glass, I'll score using my circle cutter, flip the sheet over, and apply pressure to the areas where I scored. With luck and practice, and the RIGHT amount of pressure, I will then see the back side of my score.
It's getting that scored circle to show on the back side that's the tough part. The amount of pressure and where to apply on the back of the score, that's some thing that WILL bet better with time and practice.
It's getting that scored circle to show on the back side that's the tough part. The amount of pressure and where to apply on the back of the score, that's some thing that WILL bet better with time and practice.
Deborah
After scoring the circle on light coloured opals, I use a black marker over the score line. This black lines shows up well over a light box.
On dark opals, I use the circle maker with a marker (mine comes with a separate attachment for this) and guessing as best I can where the centre is, I mark the circle on the other side. I'm always off by a bit, but it seems to work anyways.
Cheers,
Suzan
On dark opals, I use the circle maker with a marker (mine comes with a separate attachment for this) and guessing as best I can where the centre is, I mark the circle on the other side. I'm always off by a bit, but it seems to work anyways.
Cheers,
Suzan