Can't find the photo fusing posts ...

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Jane Moore
Posts: 5
Joined: Sun May 06, 2007 11:39 am
Location: UK

Can't find the photo fusing posts ...

Post by Jane Moore »

Hi

I wonder if anyone can help? I'm looking for a firing schedule to use with photo fusing paper (the kind you print with an HP printer). I'm sure this was posted previously but when I do a search what I want doesn't come up. The instructions that came with the paper don't give a schedule, it just says don't fuse over 1350F ...

Thanks

Jane :?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Can't find the photo fusing posts ...

Post by Brock »

The instructions may have been among the lost posts in the latest upgrade.
Just use a schedule appropriate for the glass you are firing on.
Jane Moore
Posts: 5
Joined: Sun May 06, 2007 11:39 am
Location: UK

Re: Can't find the photo fusing posts ...

Post by Jane Moore »

Hi

Thanks for the quick reply; I was just a bit confused because the instructions say don't fire above 1350F and for a full fuse of 2 pieces of Bullseye totalling 6mm thickness I would normally fuse to 1450F. Would I get away with just fusing to 1350F?

Thanks

Jane :)
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Can't find the photo fusing posts ...

Post by Brock »

Make your 2 layer blank first using your normal schedule and add the PF in a later, cooler firing.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Can't find the photo fusing posts ...

Post by Barry Kaiser »

We use a lot of that paper and fire in our small kiln (8x8) to 1410 on clear glass. Schedule is 0-1410 as fast a possible, hold 10...done.
Note this is for 1 layer 2x2 pieces. In our large kiln we go to 1350, hold 10...done.
I find it curious that they indicate a max of 1350. In our experience, if you fire too low, the toner does not sink into the glass far enough to hold.

Barry
Jane Moore
Posts: 5
Joined: Sun May 06, 2007 11:39 am
Location: UK

Re: Can't find the photo fusing posts ...

Post by Jane Moore »

Great, thanks for the suggestions guys, I'll give them a go.

Jane :D
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Can't find the photo fusing posts ...

Post by bob proulx »

I Fuse the glass first and fire to 1380 and hold 15. This has always worked for me.
Bob
Attachments
weeb.jpg
weeb.jpg (11.53 KiB) Viewed 18476 times
Jane Moore
Posts: 5
Joined: Sun May 06, 2007 11:39 am
Location: UK

Re: Can't find the photo fusing posts ...

Post by Jane Moore »

They're lovely Bob!
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Can't find the photo fusing posts ...

Post by bob proulx »

Jane Moore wrote:They're lovely Bob!
Thanks Jane, those are coasters with pictures of our little town. I sell them in sets of four and they sell very well.
Bob
Jane Moore
Posts: 5
Joined: Sun May 06, 2007 11:39 am
Location: UK

Re: Can't find the photo fusing posts ...

Post by Jane Moore »

Just a quick question Bob, how do you manage to get the images to go right to the edge like that ... all the instructions I've come across say you need to leave a gap ...

Jane :D
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Can't find the photo fusing posts ...

Post by bob proulx »

Jane Moore wrote:Just a quick question Bob, how do you manage to get the images to go right to the edge like that ... all the instructions I've come across say you need to leave a gap ...

Jane :D
Jane, I sent you a pm.
Bob
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Can't find the photo fusing posts ...

Post by Barry Kaiser »

Great pieces Bob,

Your detail and especially the saturation are great.

Barry
Post Reply