best glass bandsaw
Moderators: Brad Walker, Tony Smith
best glass bandsaw
I searched this forum for "best glass bandsaws" and didn't find much. Can anyone recommend a good one? I will be using it to cut from 5/8" to 1" thick glass. In my research I found three that seem possible. Diamond Laser 3000 XL got mostly favorable reviews for ease of cutting. Cons were noise, water sprays all over, uneven plastic table, flimsy construction. Cost $428.39. Denver Glass has the GS-100 and GS-60. Couldn't find reviews of either. Cost $2300 and $1250 respectively. The GS-100 looks heavy duty but it's more than I want to spend. Has anyone used the GS-60?
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: best glass bandsaw
In my opinon, by far, the best alternative is a waterjet machine. Save your tool money and hire a waterjet when you need it.
I have a Gryphon bandsaw/paperweight sitting on a shelf taking up otherwise valuable space.
I have a Gryphon bandsaw/paperweight sitting on a shelf taking up otherwise valuable space.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Re: best glass bandsaw
I do not know how well it handles thick glass
but the German Proxxon brand
http://www.proxxon.com/eng/html/27172.php
looks well built and has diamond band plus water feed.
For precice cutting of thin glass it is excellent.
very narrow kerf permits cutting both sides if a figure line in one run.
Unfortunately I do not have one, but I've seen it used.
-lauri
but the German Proxxon brand
http://www.proxxon.com/eng/html/27172.php
looks well built and has diamond band plus water feed.
For precice cutting of thin glass it is excellent.
very narrow kerf permits cutting both sides if a figure line in one run.
Unfortunately I do not have one, but I've seen it used.
-lauri
Re: best glass bandsaw
You want to cut some really thick glass- how about a tile saw? Bandsaws for glass are good for 1/4 inch, maybe.
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: best glass bandsaw
This is the saw I want next.
http://www.youtube.com/watch?v=O_VoXxL5 ... r_embedded#!
http://www.hisglassworks.com/cart/Gemin ... DuAQdaPWVo
http://www.youtube.com/watch?v=O_VoXxL5 ... r_embedded#!
http://www.hisglassworks.com/cart/Gemin ... DuAQdaPWVo
Rick Wilton
Re: best glass bandsaw
I have a Revolution XT, love it. It runs through thin and thick pieces (I've cut sheet glass to 1", including slices off that were 1/8" from a 1" thick slab), has a thin blad (slightly more than 1mm), and if you go slow, it won't break out at the end of the cut. And as the brochures say, you can cut indoors without getting water everywhere. It takes some practice to get the right amount of water in the tank (too much and you do get a lot of water on the table, which will make it's way to the floor), so follow the recommended measurement (I think 3 gallons) until you get a feel for the right amount for you.
Ed
Ed