Almost There
I've been playing around a bit with getting some multi-colored castings. This was the first practice model.
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
Richard Blummer
- Posts: 13
- Joined: Wed Jul 14, 2010 9:15 am
- Location: Egg Harbor Township, NJ
- Contact:
Re: Almost There
Looks great. Are you casting them together (or recasting with inclusions), or casting the pieces separately and gluing them in?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Almost There
Each of the characters, the barrel and the box are cast individually, then placed onto a wax base, reinvested, wax out, clear glass in.... so the piece is one solid piece, no glue. Tim
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Almost There
Beautiful and very well done.
Barry
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Almost There
I'd guess that the first practice model has you fairly excited about where it can take you, I like it. From memory this is part of the natural progression in your work, would be great to see it all at some stage when the time is right. I'm looking at the work and see how it would create much enjoyment in all the processes. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!