Almost There

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Almost There

Post by Yardic Glassworks »

I've been playing around a bit with getting some multi-colored castings. This was the first practice model.
Attachments
Band Web 2.jpg
Band Web 1.jpg
Tim Yardic
Yardic Glassworks
Richard Blummer
Posts: 13
Joined: Wed Jul 14, 2010 9:15 am
Location: Egg Harbor Township, NJ
Contact:

Re: Almost There

Post by Richard Blummer »

=D>
WOW! That's beautiful work, Tim!
=D>
אָשֵׁר חַיִּים
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Almost There

Post by Morganica »

Looks great. Are you casting them together (or recasting with inclusions), or casting the pieces separately and gluing them in?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Re: Almost There

Post by Yardic Glassworks »

Each of the characters, the barrel and the box are cast individually, then placed onto a wax base, reinvested, wax out, clear glass in.... so the piece is one solid piece, no glue. Tim
Tim Yardic
Yardic Glassworks
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Almost There

Post by Barry Kaiser »

Beautiful and very well done.

Barry
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Almost There

Post by twin vision glass »

=D> =D> =D> =D> =D> =D> =D> =D>
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Haydo
Posts: 292
Joined: Fri Mar 14, 2003 9:55 am
Location: Eimeo, Qld., Australia
Contact:

Re: Almost There

Post by Haydo »

I'd guess that the first practice model has you fairly excited about where it can take you, I like it. From memory this is part of the natural progression in your work, would be great to see it all at some stage when the time is right. I'm looking at the work and see how it would create much enjoyment in all the processes. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
Post Reply