This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.
Moderators: Brad Walker, Tony Smith
-
Terry Ow-Wing
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
-
Contact:
Post
by Terry Ow-Wing »
I'm looking for pens that will fire and can be readable for signitures or notes for test fires. I looked at
[
http://www.fusionheadquarters.com/Searc ... earch=pens]
are these good ? I'm looking mostly for the black and white and possible the gold pen to add details to pendants. Any advice will be appreciated.

-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
-
Contact:
Post
by Barry Kaiser »
Try the pilot silver markers...available at Staples (for some reason not available at Office Depot).
Inexpensive and they do withstand firing.
Barry
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Post
by Kevin Midgley »
Bic white out pen