I slumped over a stainless mold with too hot a temperature. Some of the glass is baked on. Is there way to remove the stuck glass from the stainless mold?
Thanks in advance,
Carol Ann
removing glass from stainless steel mold
Moderators: Brad Walker, Tony Smith
removing glass from stainless steel mold
Carol Ann
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: removing glass from stainless steel mold
get it hot and dump into water. rosanna
artist, owner of wanchese art studio, marine finisher
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: removing glass from stainless steel mold
use eye protection. rosanna.
artist, owner of wanchese art studio, marine finisher
Re: removing glass from stainless steel mold
Rosanna,
Will it not explode? or this is the reason for the safety glasses?
thanks,
Havi
Will it not explode? or this is the reason for the safety glasses?
thanks,
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: removing glass from stainless steel mold
it might pop and steam but not explode. safety glasses are cheap and easy insurance. i got a piece of glass in my eye a couple of weeks ago doing something stupid. i was lucky. i washed it out with no harm. safty glasses or a face shield thet took all of 2 seconds to put on would have saved me alot of angst. rosanna
artist, owner of wanchese art studio, marine finisher
Re: removing glass from stainless steel mold
glad to hear you are OK now!
havi
havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: removing glass from stainless steel mold
Thanks Havi and Rosanna,
I will wear safety glasses and face shield. Thanks for the information
Carol Ann
I will wear safety glasses and face shield. Thanks for the information
Carol Ann
Carol Ann