Anyone have experience with Loctite Durabond 530CL?
Thanks!
Loctite Durabond 530CL- reviews?
Moderators: Brad Walker, Tony Smith
-
Bonnie Rubinstein
- Posts: 239
- Joined: Sun May 04, 2003 9:04 pm
- Location: River Falls, WI
Loctite Durabond 530CL- reviews?
Bonnie Rubinstein
-
Bonnie Rubinstein
- Posts: 239
- Joined: Sun May 04, 2003 9:04 pm
- Location: River Falls, WI
Re: Loctite Durabond 530CL- reviews?
Just found out that product name was dropped- it is now Loctite E-30CL.
Bonnie Rubinstein
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Loctite Durabond 530CL- reviews?
I've used it. It's a strong epoxy. It's water clear. It requires a special applicator that costs more than the glue. It's not super thin, so it's hard to hide the bondline.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun