Grade of stainless steel for molds?
Moderators: Brad Walker, Tony Smith
Grade of stainless steel for molds?
What kind of stainless steel is used for molds? 306? 304?
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Grade of stainless steel for molds?
I use 304 stainless for my molds. I sometimes fire my molds quite hot, like in the high 1400's, and they still work fine. 304 is the most common grade of stainless steel. There are grades that are rated hotter, but you don't need to spend extra for that.
Bert
Bert Weiss Art Glass*