I like Amazing Glazing line of bits from CR Laurence. I have bought some cheap Chinese bits, but they turned out to be nearly useless to me because they were too short for my tripod drill setup. The AG bits cost a little more and last a lot longer, than their EDD series.Bonnie Rubinstein wrote:I started with the base being single thick, then added on layers, so it became DT..except in a few areas.
I have had luck with the DT to start with, and if it were not for the weight, I would have used DT for this as well. But then I would have added more glass, making it very thick, and for this fixture, I wanted it to be a little lighter. I think I should have added enough glass to make the whole piece DT, consistently.
.. and Bert, if you have a good source for hollow core bits that LAST, please inform..
thanks!
Surprise crack
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Surprise crack
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Surprise crack
If the crack is where it will not be seen maybe you could drill small holes at the ends of the crack to stop them form spreading. I still would not sell it but it may buy you time to show it.
Bob
Bob
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Surprise crack
if you hang it in your kitchen like you suggested, you may be awaken some night by a huge crash