Gondwana Banana
A while back (must be nearly 2 years) I was making a multi media piece which incorporated glass, wood & bronze. I promised Morganica among other people that I would post a picture when it was completed. It has now been installed in a sculpture exhibition in NZ called NZSoS (New Zealand Sculpture onShore).
Originally it had a bunch of glass fruit cast as one piece. I was not happy with it & attempted to refire it with disastrous results. The glass components have now all been cast separately.
Here it is:
You can see many more images on my Facebook page.
Cheers,
Ron
Originally it had a bunch of glass fruit cast as one piece. I was not happy with it & attempted to refire it with disastrous results. The glass components have now all been cast separately.
Here it is:
You can see many more images on my Facebook page.
Cheers,
Ron
Re: Gondwana Banana
That is absolutely gorgeous.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Gondwana Banana
Obviously good things take time; this is stunning!
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Gondwana Banana
Now we know where you have been and the waite has been sooooooo very worth it. Amazing, fantastic , wonderful and well, simply stunning.
Leslie
Leslie
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
Re: Gondwana Banana
Wow - it's beautiful!
Barb
Barb
Re: Gondwana Banana
Boy, did THAT come out well. It begs to be stroked--lovely, lovely coldworking.
So what were the disastrous results from the refiring?
So what were the disastrous results from the refiring?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Gondwana Banana
Beautiful Pieces and the Total is spectacular.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Ron Reichs
- Posts: 4
- Joined: Sat Oct 09, 2004 2:02 am
- Location: New Zealand
- Contact:
Re: Gondwana Banana
Thanks all for your kind comments.
First I'll tell you about the disastrous refiring of the bunch of fruit.
It was done in Bullseye cranberry. After coldworking the piece I was not happy with the excessive amount of bubbles (half bubbles) on the surface of the glass withe many more below the surface. If I coldworked the surface ones off, more would appear so I resolved to refire it in an attempt to eliminate as may of these as possible. After filling the surface bubbles with wax, I reinvested the glass & refired with a long soak at 830c
(16hrs) Unfortunately on the downwards ramp, the mould cracked & leaked half the contents over the kiln floor. This wouldn't have been so bad if I could have reclaimed most of it, remade the piece & topped up with new glass to replace that which was lost.
Unfortunately Bullseye cranberry is a striker & on the second firing it had gone liverish so no hope of using any of it again especially for a third firing.
With the new work I made each banana as a separate unit so I was able to use Bullseye amber on two of them & Gaffer orange red for the other two.
To eliminate bubbles I cast these horizontally in open faced moulds & carved off the excess glass after firing.
The results were much more pleasing.
I'll make another post to give the specs of thework.
Cheers,
Ron
First I'll tell you about the disastrous refiring of the bunch of fruit.
It was done in Bullseye cranberry. After coldworking the piece I was not happy with the excessive amount of bubbles (half bubbles) on the surface of the glass withe many more below the surface. If I coldworked the surface ones off, more would appear so I resolved to refire it in an attempt to eliminate as may of these as possible. After filling the surface bubbles with wax, I reinvested the glass & refired with a long soak at 830c
(16hrs) Unfortunately on the downwards ramp, the mould cracked & leaked half the contents over the kiln floor. This wouldn't have been so bad if I could have reclaimed most of it, remade the piece & topped up with new glass to replace that which was lost.
Unfortunately Bullseye cranberry is a striker & on the second firing it had gone liverish so no hope of using any of it again especially for a third firing.
With the new work I made each banana as a separate unit so I was able to use Bullseye amber on two of them & Gaffer orange red for the other two.
To eliminate bubbles I cast these horizontally in open faced moulds & carved off the excess glass after firing.
The results were much more pleasing.
I'll make another post to give the specs of thework.
Cheers,
Ron
-
Ron Reichs
- Posts: 4
- Joined: Sat Oct 09, 2004 2:02 am
- Location: New Zealand
- Contact:
Re: Gondwana Banana
Here are the specs. of Gondwana Banana:
Height: 2500mm
Width: 500mm
Materials:
Glass: Leaf bud: Bullseye casting billet amber 3.8kg
Banana x 2: Bullseye casting billet amber 3.6kg each
Banana x 2: Gaffer lead crystal orange red 5.1kg each
Total glass: 21.2kg
Wooden pole: jarrah (Australian hardwood) 1670 x 180 x 180 36kg
Silicon Bronze
Crown: 950 x 500 x 500 17kg
Roots: 950 x 450 x 450 17.5kg
Total bronze: 34.5kg
Cheers,
Ron
Height: 2500mm
Width: 500mm
Materials:
Glass: Leaf bud: Bullseye casting billet amber 3.8kg
Banana x 2: Bullseye casting billet amber 3.6kg each
Banana x 2: Gaffer lead crystal orange red 5.1kg each
Total glass: 21.2kg
Wooden pole: jarrah (Australian hardwood) 1670 x 180 x 180 36kg
Silicon Bronze
Crown: 950 x 500 x 500 17kg
Roots: 950 x 450 x 450 17.5kg
Total bronze: 34.5kg
Cheers,
Ron
Re: Gondwana Banana
I just think this is one of the best pieces I have seen in years . . . amazing.
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Gondwana Banana
It is an amazing piece.
Bob
Bob
-
Warren Weiss
- Posts: 137
- Joined: Thu Mar 13, 2003 8:06 pm
- Location: Richmond, VA
Re: Gondwana Banana
Beautiful.
Warren
Warren
Re: Gondwana Banana
Chapeau
and
Congrats,Ron.
I remeber you said you put some hundreds of hours of polishing...............
one can see the results!
Havi
and
Congrats,Ron.
I remeber you said you put some hundreds of hours of polishing...............
one can see the results!
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com