What are some recommended texts for techniques on deeply slumping vessels? For example, how to slump bell-shaped objects?
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Resources for deep slumping?
Karl Harron, from Northern Ireland, has developed molds and techniques for this. He has been teaching at a few studios around the USA. I believe you can purchase a set of Karl's molds from Bullseye, and probably at studios where he has taught, like Weisser Glass in MD. He did quite a bit of R&D to come up with a multi-mold technique. He decided to sell the molds with the R&D factor built in to the cost of the molds. I think that means they are a fantastic bargain. I have spoken with students in his classes, and they were thrilled for the opportunity to learn from Karl's experiences.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
- Posts: 57
- Joined: Sun Dec 13, 2009 9:35 pm
Re: Resources for deep slumping?
Thanks for the reference, I will go a-snoopin' about for his stuff.
UPDATE: Thanks a lot, Bert. Now I have a new artist to obsess over.
UPDATE: Thanks a lot, Bert. Now I have a new artist to obsess over.
-
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Resources for deep slumping?
Where are the molds? I couldn't find them at either place you suggested.
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
- Posts: 57
- Joined: Sun Dec 13, 2009 9:35 pm
Re: Resources for deep slumping?
I found references to them in some of the Bullseye blog posts. Here's instructions, which seem *very* useful. I might try to make some of my own based on these . . . paying especial attention to the proportionate shifts in diameter and depth at each step.The Hobbyist wrote:Where are the molds? I couldn't find them at either place you suggested.
Jim
http://www.creativeceramics.eu/docs/slu ... _steps.pdf
And here's Karl's stuff . . . there's no doubt but that he is a phenomenal talent: http://www.theglasstudioireland.com/gallery_1.html
(Be sure to view all four galleries.)
-
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Resources for deep slumping?
And so where does own go to obtain the molds?
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Re: Resources for deep slumping?
Check under distributors
-
- Posts: 57
- Joined: Sun Dec 13, 2009 9:35 pm
Re: Resources for deep slumping?
There's this fantastic resource called an Internet Search Engine. You should totes check it out.The Hobbyist wrote:And so where does own go to obtain the molds?
Jim

Re: Resources for deep slumping?
You can buy the molds at Creative Ceramics.
On their website you have also the instructions how to use them.
Karl teaches also intensively in Europe too....................
Havi
On their website you have also the instructions how to use them.
Karl teaches also intensively in Europe too....................
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile

"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com