Bohle Silberschnitt running pliers

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Bohle Silberschnitt running pliers

Post by Mark Wright »

Image
I recently bought a pair of Bohle running pliers and they seem worthless. I cannot get a score to run without excessive pressure which causes a “bullseye” to chip out on the back side. Bullseye Glass (where I ordered them) says I am squeezing too hard and they are right, but any less pressure and the score does not run. Has anyone else experienced problems with these pliers? Maybe they are defective? I cannot see anything wrong with them except they do not have a curved jaw to work against like my other running pliers.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Bohle Silberschnitt running pliers

Post by Brock »

I had a pair and quickly abandoned them. Overpriced and inefficient.
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Bohle Silberschnitt running pliers

Post by AndyT »

I've been using the same pair of cheap Taiwan runners for 30 years and they work great. About $15 or so retail.

Andy
JenniferB
Posts: 61
Joined: Mon Jan 17, 2005 9:15 am

Re: Bohle Silberschnitt running pliers

Post by JenniferB »

I, too, bought a pair and found them very difficult to use. Like you, I had to squeeze far too hard but had no success with lighter pressure. They sit in the back of a drawer doing nothing, while I use a pair of inexpensive running pliers.
Jennifer
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Bohle Silberschnitt running pliers

Post by Morganica »

I use both, but for different thicknesses of glass. The standard (cheaper) running pliers work well, and certainly work for both, and are better on thicker glasses. I find the Bohles are better on difficult-to-break glass (such as pale opals) since they break more slowly and let you control the run. They also tend to make very clean, fast runs on thin glass where the harder pliers might produce a crooked or slightly chipped edge (for me, at least). I like them for breaking out lots of small circles when I'm using the lenscutter on thin glass (and especially into irid, where a ding in the coating will show).

But no, unless I had a specific reason to buy them (i.e., lots of thin irid circles)..I don't know that I'd buy them again.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Bohle Silberschnitt running pliers

Post by Havi »

I also put this pliers aside, because of bad functioning.





Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Bohle Silberschnitt running pliers

Post by Morganica »

Well...I don't think they're bad at all. I quite like them, but they have a learning curve. They don't need all that much force, but you need to be patient about running the score without pressing too hard.

I'm just not sure that most glass cuts require that much finesse...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Bohle Silberschnitt running pliers

Post by Valerie Adams »

I bought them from a seller on Ebay, thinking I was making a score (no pun intended) because they were so inexpensive. Used them a few times and was glad I didn't pay retail. I also use the cheap running pliers; same pair for the last 11 years. I finally replaced the rubber tips.
Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Re: Bohle Silberschnitt running pliers

Post by Lauri Levanto »

Most running pliers have curved jaws. They are good.
Bohle has a flat upper jaw and a tiny nibble in the middle of the bottom jaw.
I made a little groove n the upper jaw surface that matches the nibble.
That works.
-lauri
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Re: Bohle Silberschnitt running pliers

Post by Mark Wright »

Now my question is what to do with a pair of worthless pliers. I think I will pack them up and send them to Brad Walker. Perhaps he will favor us with his opinion.

Brad,
Feel free to keep them or whatever you wish. They have no value to me.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Bohle Silberschnitt running pliers

Post by Morganica »

Hey--send them to me. ;-)

Seriously, they're just a different way to run the break slowly and stay in control. I wouldn't call them worthless, just specialized:

Would I use them on thick glass? Nope. If it does break, it'll take forever.

Would I use them on 3mm glass? Maybe, depends on whether or not I've got some inside curves in this score and I want the glass to break very precisely on those curves. If the score hangs up, I can easily stop and attack it from a different angle. (that's one thing I do like very much about this tool--you can twist the top rubber bar to become exactly perpendicular to the tangent of the score, which comes in handy if the glass is in the way of the plier handles.

Would I use them on thin glass? Every time. The glass breaks cleaner, without the usual slanty or chipout direction at the point of the break.

The trick, as I said, is to keep the pressure firm but light, and be patient. If all you're doing is breaking 3mm sheet, mostly straight, you don't need them.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Bohle Silberschnitt running pliers

Post by Valerie Adams »

Morganica wrote: Would I use them on thin glass? Every time. The glass breaks cleaner, without the usual slanty or chipout direction at the point of the break.
OK; I'm going to put mine out on my workbench and try them for thin glass!
grozier
Posts: 10
Joined: Sat Jun 04, 2005 5:44 pm
Location: Charlotte, NC
Contact:

Re: Bohle Silberschnitt running pliers

Post by grozier »

I find them very helpful when breaking out thin strips of 1/4" or less when working with 3mm glass.
Faye Malench
Posts: 46
Joined: Sun Jan 02, 2005 9:03 pm
Location: Illinois
Contact:

Re: Bohle Silberschnitt running pliers

Post by Faye Malench »

I cut a lot of long narrow strips and this is the last tool I would use. The glass chips away where the pliers are applied and more flares on the ends of the score. It does not work for me on thins and thin dichro either. For 3 to 9 mm I use my regular running pliers. For a lot of single layer narrow strips I use a smaller version of regular running pliers - I think it is a Dragon tool. It's small and fits my hand. The head is aligned so it fits perfectly for 1/4 inch strips, though I can get 1/8 with a small margin of breakage.

I like Bohle products normally - I bought the running pliers based on the rave reviews of a wgb member and was disappointed. Never thanked him for that.
Mary Kay Nitchie
Posts: 21
Joined: Mon Mar 10, 2003 8:02 pm
Location: Portland, Oregon
Contact:

Re: Bohle Silberschnitt running pliers

Post by Mary Kay Nitchie »

Hi all,

Bullseye recommends the Bohle pliers for inside curves and thin strips, not for most cutting tasks.

We ran this thread by Janet, long-time manager of the Bullseye Resource Center. She sent me an email, saying,
In my experience with these pliers, Cynthia’s evaluation is spot on. Most of the time the inexpensive Running Pliers (7008) are all you need and are the best tool for the job. The Bohle Pliers are a useful tool under circumstances she mentions, where you wouldn’t use the Running Pliers (7008) pliers.
So, using the right tool for the right job is part of the solution. And if you can only buy one set of running pliers, go for the standard ones. And replace the pads when the pads wear out.

Mary Kay
Mary Kay Nitchie
Bullseye Glass Co.
http://www.bullseyeglass.com
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Bohle Silberschnitt running pliers

Post by Bert Weiss »

Regardless of which pliers you use, the best strategy for strip cutting is to cut the glass in half. So, you might start out with a 4" piece. Cut it in to 2" pieces, then 1" pieces etc. When you do this, you will notice the flare gets evened out by the opposite stresses.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Phil Hoppes
Posts: 298
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Re: Bohle Silberschnitt running pliers

Post by Phil Hoppes »

I do a fair amount of strip work and these work like a champ. Never had an issue with them and most of the time work far better than anything else I've ever used. For irregular shape cuts, probably not. For strips, their the bomb and worth every penny.
Post Reply