Wanted: Source for 19" Bottle Slumping Molds

Post by David Jenkins »

Our neighbor has some bottles she'd like slumped into a mold. The bottles are very tall (19 in.) blue glass Riesling bottles, with a narrow shoulder (brand unknown). None of the molds I've seen from some Googling are quite that long. I am not at all into bottle slumping, but have told her I'd try a couple for her if she bought the mold - does anybody know of a source for a mold that will accommodate such a tall bottle?
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Wanted: Source for 19" Bottle Slumping Molds

Post by JestersBaubles »

David,

I came across an 18.5" bottle slumper today while looking for something else:

http://www.americanglasssupply.com/html ... molds.html

It's ACSC176 Large Bottle Sagger.

Dana W.