Papyros fiber paper
Moderators: Brad Walker, Tony Smith
Papyros fiber paper
Hi everyone and Happy Thanksgiving,
Has anyone used the Papyros fiber paper. Pros/Cons?? I use Bullseye thinfire all the time, and buy it in the 200 20.5 x20.5 sheet pack. I like the idea of the Papyros as it comes in a studio roll or a craft roll - within my budget. I just can't buy the Bullseye roll even though it would probably last me for years. I wish it came in smaller rolls.
Any comments are appreciated. Thanks.
Patty
Has anyone used the Papyros fiber paper. Pros/Cons?? I use Bullseye thinfire all the time, and buy it in the 200 20.5 x20.5 sheet pack. I like the idea of the Papyros as it comes in a studio roll or a craft roll - within my budget. I just can't buy the Bullseye roll even though it would probably last me for years. I wish it came in smaller rolls.
Any comments are appreciated. Thanks.
Patty
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
-
Alexis Dinno
- Posts: 57
- Joined: Sun Dec 13, 2009 9:35 pm
Re: Papyros fiber paper
It does. I have bought one in the local Bullseye store. Get on the phone to Bullseye.Pat K. wrote:I wish it came in smaller rolls.
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Papyros fiber paper
I'm not sure what you mean by smaller rolls. Bullseye thinfire comes in a small roll that is 10 feet by 41 inches. The small Papyros "studio roll" is 33 feet by 41 inches.Pat K. wrote:I use Bullseye thinfire all the time, and buy it in the 200 20.5 x20.5 sheet pack. I like the idea of the Papyros as it comes in a studio roll or a craft roll - within my budget. I just can't buy the Bullseye roll even though it would probably last me for years. I wish it came in smaller rolls.
-
Doug Randall
- Posts: 102
- Joined: Sun Aug 17, 2003 10:11 pm
- Location: Portland, OR
- Contact:
Re: Papyros fiber paper
Several years ago I bought a few rolls of "thin fire" like paper from a company that someone here on the board recommended and had posted the URL for.
I can no longer find their link on my computer or by doing a WGBB search. If anyone knows of this company and their site, could you please post the link.
This paper was not the greatest for firing at a full fuse but it worked well for my low and slow process.
I can no longer find their link on my computer or by doing a WGBB search. If anyone knows of this company and their site, could you please post the link.
This paper was not the greatest for firing at a full fuse but it worked well for my low and slow process.
-
Lynn Perry
- Posts: 129
- Joined: Sun Jun 08, 2003 5:27 pm
- Location: East Tennessee
Re: Papyros fiber paper
Doug, it may have been this:Doug Randall wrote:Several years ago I bought a few rolls of "thin fire" like paper from a company that someone here on the board recommended and had posted the URL for.
I can no longer find their link on my computer or by doing a WGBB search. If anyone knows of this company and their site, could you please post the link.
This paper was not the greatest for firing at a full fuse but it worked well for my low and slow process.
http://www.techniglassstore.com/cat-kiln-liner.cfm
I used it for a while and had some strange problems. Just trashed 50 sheets a couple of weeks ago....
Lynn Perry
-
Doug Randall
- Posts: 102
- Joined: Sun Aug 17, 2003 10:11 pm
- Location: Portland, OR
- Contact:
Re: Papyros fiber paper
Thats the one. Thanks for the link Lynn
Re: Papyros fiber paper
Thanks everyone - I really didn't check the archives. I didn't even think about them. I also didn't realize that the Bullseye came in the 10' x 41" roll either. I had only seen it in the big roll that costs 900+ which, of course, I can't/won't purchase at one time. I appreciate your not taking me to task for my oversight.
Patty
Patty
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
Re: Papyros fiber paper
I recently bought a few sheets of Papyros from Delphi Glass http://www.delphiglass.com/fusing-suppl ... aper-sheet
I prefer to use kiln wash, but will occasionally use thin fire. I was drawn to the claim that this paper can be reused, but after firing something at full-fuse temperature, it pretty much fell apart where I touched it. Also, I agree that it leaves too much texture.
I'd suggest if anyone wants to give it a try, to buy a sheet first. There are some good reviews of this out there (beyond the one on Delphi), so apparently other folks have different experiences. I'm glad I didn't invest more money into this for my personal use.
I prefer to use kiln wash, but will occasionally use thin fire. I was drawn to the claim that this paper can be reused, but after firing something at full-fuse temperature, it pretty much fell apart where I touched it. Also, I agree that it leaves too much texture.
I'd suggest if anyone wants to give it a try, to buy a sheet first. There are some good reviews of this out there (beyond the one on Delphi), so apparently other folks have different experiences. I'm glad I didn't invest more money into this for my personal use.