Hello all.

I've crushed some frit. The average is the size of rice grains. Then ran a magnet through it.

Then I washed it in a weak soap and water solution then rinsed in water.

The frit holds a lot of water! Waiting for the water to evaporate takes forever.

How do I dry the frit?

Peter
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: How to dry frit

Post by Buttercup »

Peter, can you put it in the kitchen oven, if there's already something in your kiln? Just on low, enough to evaporate the moisture? Jen
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: How to dry frit

Post by Greg Rawls »

Spread it out on a window screen and put in the sun for a few hours.
Greg
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: How to dry frit

Post by Morganica »

So this is gonna sound dumb, but go to the Goodwill or its equivalent and see if you can find an old salad spinner. Put the frit in the salad spinner, pump the thing like crazy, and you'll drive off most of the water. (Obviously, don't do this with the REAL salad spinner you use in the kitchen--you'll get glass grit in your greens for weeks, the stuff is insidious).

Once you've done that, spread it on Greg's screen, or a cookie sheet with layers of parchment paper, and either hit it with a blowdryer, put it in the oven, put it on top of your firing kiln, or just leave it alone for a few days. (In Oregon, the sunny thing isn't an option, at least not right now) ;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: How to dry frit

Post by Peter Angel »

Dear all. Thanks for all your ideas.
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: How to dry frit

Post by Laurie Spray »

I would personally not wash it......but if you really feel the need i would spred it on cookie sheets and dry on a firing kiln. Stir after a few hours. Be sure to screen out the glass dust.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: How to dry frit

Post by Bert Weiss »

I put it in a stainless steel bowl in the kiln. Heat the sucker right up. Water gone.

I don't think I would use soap on it though.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Petra Kaiser
Posts: 9
Joined: Mon Mar 17, 2003 5:46 pm
Location: Cape Coral, FL
Contact:

Re: How to dry frit

Post by Petra Kaiser »

I like washing my frit, too then I apply it wet to the glass and let it sit to dry in the kiln room over night. If you use it for castings then I would dry it spread out thin on clean sheets of glass covered with some newspaper over night.
petra kaiser, florida,

"Have no fear of perfection, you'll never reach it" -Salvador Dali-

specialized in kiln forming with Kaiser Lee Board since 1998
http://www.kaiserlee.com
Drake
Posts: 2
Joined: Sat Feb 23, 2013 12:29 pm

Re: How to dry frit

Post by Drake »

If you are going to use the glass for casting it will dry out in the mold, or in the flower pots before it melts into the mold.
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: How to dry frit

Post by Marian »

I agree with Bert, soap is likely to cause contamination issues. Heat your bowl of frit- fast as you can is fine, -up to 450 hold 15 or 20 minutes- done. Yes, you could heat it in the oven if your kiln is too small or in use.
Laurie Saukko
Posts: 13
Joined: Tue Mar 13, 2012 12:57 pm

Re: How to dry frit

Post by Laurie Saukko »

toaster oven, great for small batches.
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: How to dry frit

Post by Peter Angel »

I did try drying frit in a toaster oven but when I cast the glass I got really bad devit. So bad the glass surface was wrinkled. A bit like my fingertips after a long bath.
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Jerrwel
Posts: 129
Joined: Thu Feb 10, 2005 6:25 pm
Location: Charlotte, NC

Re: How to dry frit

Post by Jerrwel »

Peter Angel wrote:Hello all.

I've crushed some frit. The average is the size of rice grains. Then ran a magnet through it.

Then I washed it in a weak soap and water solution then rinsed in water.

The frit holds a lot of water! Waiting for the water to evaporate takes forever.

How do I dry the frit?

Peter
I put my 'rinsed' (no soap) frit in a pyrex bowl, cover loosely and microwave. Done.
Jerry
Post Reply