With clear casting using Resins, a method to remove bubbles is to saturate the surface of the liquid resin with Carbon Dioxide, CO2.
I do not know how it works but it does work.
Has anyone tried infusing CO2 into the kiln to remove bubbles from the hot glass.
removing bubbles
Moderators: Brad Walker, Tony Smith
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: removing bubbles
A reducing environment will frig up your elements. The resin thing is as much a function of heat as co2. Rosanna
artist, owner of wanchese art studio, marine finisher
-
Beau Lyons
- Posts: 32
- Joined: Fri Sep 21, 2012 11:47 pm
Re: removing bubbles
I will check with kiln manufacturers,
I have been informed it is not a function of heat.
I have been informed it is not a function of heat.