I am thinking about getting a ring saw to cut irregular shapes out of standard thickness System 96.  What is the current consensus regarding the saws that are presently on the market?
Thanks,
Terry
			
			
									
						
										
						Current info on ring saws
Moderators: Brad Walker, Tony Smith
- 
				Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: Current info on ring saws
I use the Taurus 3 - it works fine for 3mm glass.   I've also cut thicker (up to 3 layers) - it's very hard on the blade, but it will do it.   
Barb
			
			
									
						
										
						Barb
- 
				bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Current info on ring saws
I have the Tauras 3, good tool.
Bob
			
			
									
						
										
						Bob
Re: Current info on ring saws
Reviewed the Taurus III several years ago, but the review's still valid:
http://www.morganica.com/bloggery/2007/ ... -ring-saw/
			
			
									
						
							http://www.morganica.com/bloggery/2007/ ... -ring-saw/
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Current info on ring saws
i use the taurus 3 for production, depending on what i'm doing i use either the speed blade - so far the longest lasting - or the mega blade.  the standard blade is for single thickness - up to 3mm - only or you can break it - yes, i've broken 2 way back.  despite the plastic used, it's held up well for 7 or 8 yrs now.
D
			
			
									
						
										