hey
 I remember someone mentioning purchasing MR-97 buy the case at a much cheaper price than my retail store at $50. a can... I can't find the thread.  I would appreciate some help in finding the source... I love the stuff!  If I remember correctly it was much less than 1/2 the price if you purchase by the case.  
thanks in advance Janet
			
			
									
						
							purchase MR-97
Moderators: Brad Walker, Tony Smith
- 
				Janet McFadyen
 - Posts: 48
 - Joined: Mon Aug 28, 2006 4:40 pm
 - Location: Vancouver Island, BC
 
purchase MR-97
facebook artist page @ Janet McFadyen's Glass
			
						Re: purchase MR-97
I hope you don't my hi-jacking this post with a question about how you use MR-97?
Once you have sprayed it on a mold and slumped or draped with it, does the mold need cleaning and/or re-spraying?
I have some small molds I use for casting with frits and powders. I broke some by using primo primer, and learned later that I needed the MR-97.
Thanks,
Loraine
			
			
									
						
										
						Once you have sprayed it on a mold and slumped or draped with it, does the mold need cleaning and/or re-spraying?
I have some small molds I use for casting with frits and powders. I broke some by using primo primer, and learned later that I needed the MR-97.
Thanks,
Loraine
- 
				Janet McFadyen
 - Posts: 48
 - Joined: Mon Aug 28, 2006 4:40 pm
 - Location: Vancouver Island, BC
 
Re: purchase MR-97
after the intial 2 coats.. you only need one coat to refire
			
			
									
						
							facebook artist page @ Janet McFadyen's Glass