Hello every body,
So I made another melt.....
I want to do strip fusing around it and have a complete piece.
The piece's size is 27c'm by 23 c'm, 6 milimeter thick.
I would like to go again as high as 1700 degrees, as I like the way the glass becomes at this high temp. My hesitation is whether it will not have bad effect on the melt - by taking it again to such high temp.
Anybody with experience in this? Should I take the risk, or not?
as usual, many thanks in advance,
Havi
REFiRING MELT ON HIGH TEMPRATURE
Moderators: Brad Walker, Tony Smith
REFiRING MELT ON HIGH TEMPRATURE
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: REFiRING MELT ON HIGH TEMPRATURE
Oh dear, I am not sure Havi to take such a chance . It is soooooo lovely now. That is really hard on glass. Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
Re: REFiRING MELT ON HIGH TEMPRATURE
I have taken pieces up that high for multiple firings. As long as they didn't color shift the first time I have not had a problem. However the piece will flow along with the new glass you are adding so it will change. I am confused on what you are trying to do as an end result.