Element support rods

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Element support rods

Post by Terry Gallentine »

Does anybody out there have a good source for rods (probably mullite) used for supporting kiln elements from a kiln ceiling?
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Element support rods

Post by Rick Wilton »

http://www.duralite.com/kiln-furnace-studio.htm

Duralite sells them, you may want to consider the quartz tubes, that's what I've used in the kilns I've made.
Rick Wilton