drilled holes in pots look black

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

drilled holes in pots look black

Post by Bonnie Rubinstein »

I am about to do a pot melt with 3 small standard looking red clay pots, bought at Menards. When I drilled the extra holes, the material did not behave like clay, was harder, and was almost black. I would assume clay would have a diferent color and consistency. The residue that I get by wiping these holes is also black. I do not want the glass to pick up this black residue. Has anyone used this type of clay pot successfully?

Thanks!
Bonnie Rubinstein
Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: drilled holes in pots look black

Post by Cheryl »

nope. weird.
"Every artist was first an amateur."

--Ralph Waldo Emerson
Jim Murphy
Posts: 28
Joined: Mon Mar 10, 2003 12:39 pm
Location: IL

Re: drilled holes in pots look black

Post by Jim Murphy »

Hi Bonnie, there's a remote chance these pots are made of resin rather than clay. Perhaps a simple match flame test will be in order to determine
if the material melts and/or burns. Have water nearby.

If the pots don't melt/burn, they may indeed be made of clay and you're seeing "black-coring" which happens when iron-containing clays are improperly fired.

Good luck,

Jim
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: drilled holes in pots look black

Post by Bonnie Rubinstein »

thanks.. I shall test it.
Bonnie Rubinstein
Post Reply