OMG, is there a way not to lose it completely?
photos will follow - - -
OK, back to work,
Hi guys,
MY final goal is to fuse meshmelt piece into crakled piece which i had done separately previously.
1. Took a rectangular 3 m'm piece of fiber. Drew on it a triangle and sprinkled it with powder. Wet it as necessary, broke it, as necessary - in order to make the crackles. then put on top of it a rectangular piece of glass.
it Broke
Is it a thermal shock??
![Confused :?](./images/smilies/icon_confused.gif)
In other words - next time if I want to repeat this procedure - should I do the powdered - would be crakled part separately, and then fuse it to the general background??
2. Upon cleaning the crackled face, I realised that actually it could be fused like this. Of course cleaned and handled peoperly. And then, fuse the melt on top of it....
What do you think?
Have you got any advice / experience thatr you can share?
I'd be more than grateful.
Havi